Silver-Based Brazing Alloys |
|
|
The capability of main products:
|
|
| Item |
Melting
temperature (¡æ) |
| AgCuIn30-5 |
770-800 |
| AgCuIn27-10 |
685-730 |
| AgCuIn24-15 |
630-705 |
| AgCuSn27-5 |
730-755 |
| AgCuSn30-10 |
590-718 |
| AgCuSn28-10 |
650-700 |
| AgCuSn23-10 |
600 |
| AgCuSn32-15 |
670-690 |
|
|
|
Gold-Based Brazing Alloys
|
|
|
The capability of main products:
|
|
| Item |
Melting
point (¡æ) |
Flowing
point (¡æ) |
| AuCu20 |
908 |
910 |
| AuCu37.5 |
930 |
940 |
| AuCu50 |
955 |
970 |
| AuCu60 |
980 |
1000 |
| AuCu62.5 |
985 |
1005 |
| AuCu65 |
990 |
1010 |
|
|
|
Palladium-Based Brazing Alloys
|
|
|
Brazing Alloys for Electro-Vacuum Parts
|
|
|
Special Brazing Alloys for Semiconductor Components
|
|
|
Shinning Copper-Based Brazing Alloys with Low Silver Content
|
|
| Item |
Melting
point(¡æ) |
characteristic |
| Ag15P5Cu |
640-915 |
The plastic is high, the melting point is low, largely used in dynamo industry for brazing |
| Ag5P6Cu |
655-800 |
Soldering copper and copper alloys, largely used in dynamo, refrigerator, glasses and electric apparatus, etc. |
|
|